Softouch Super White
| Overview |
Softouch Super White are 100% waterbase low resin ink base that is APEO free, formaldehyde free Organotin
compound free and heavy metal free. The physical of the ink are White and a have excellent opacity for printing
on dark as simulated discharge printing with excellent handling.
This ink are a ready for use and can be screen or
roller printed. The finish print image are breath through and have excellent color brilliancy. It also promotes
excellent chemical resistance properties with excellent wet and dry crocking fastness result
[3.5 ~4.5].
|
|
| |
| Type Of Fabrics |
Cotton, Blends Cotton Polyester, Blend Rayon Polyester, Rayon and Polyester
*** ALWAYS PRETEST FASTNESS PROPERTIES BEFORE PRODUCTION. ***
|
|
| |
| Application Method |
White Printing
Use Softouch Super White direct from the can and if opacity on dark ground fabric are not achieve certain
percentage of Softouch White 76/769 are recommended to be added.
Color Printing
Proportionate ratio of Softouch Super White, Softouch White 76/769 and concentrated Pigment are to be are
recommended for desire opacity as well as color density. Maximum Pigments Concentrated is approximately up
to 10 % by weight for the desire colors. RFU 150 LC is recommended to be use as tinting base for desire light
colors.
|
|
| |
| Type Of Stencil & Mesh |
Used only water resistant, direct in direct emulsion. Capillary film are recommended for fine details printing (Call
your emulsion supplier for water resist emulsion)
49T to 53T mono-filament for high glossiness, Metallic, Glitter, and Shimmer.
50T to 61T mono-filament for soft hand with medium glossiness.
59T to 120T mono-filament for detail print or for fine line and tone on fabric.
|
|
| |
| Squeegees And Printing Table |
| For excellent glossiness and opacity, squeegee with 55/65 sore hardness are recommended. Soft tables are most
suitable. We suggest silicon rubber table blanket, are to be place on top of the printing pellet to improve the
printing table hardness. For special effect 65/75 sore hardness squeegee perform the best. Squeegee hardness of
75/85 was recommended for fine detail printing. |
|
| |
| Drying And Polymerization |
| For maximum fastness, prints are to be cure at 130 degree Celsius or 270 degree Fahrenheit. Airflow
recommended is 1500 cfm for proper polymerization at 3 minutes. Improper curing will cause poor fastness
properties.
|
|
| |
| Tools And Additive |
Cold Cure Catalyze (C3) is recommended at 0.1% to 1% to improve dry film cross linking properties for Softouch
System.
To improve printability of ink, Retarded W7W (W7W) is recommended to be added at 0.5% to 1.5% to the
Softouch ink system. W7W will prevent screen blocking with excellent result. This product is strongly
recommended for Automatic presses as well as for rotary cylinder printing.
|
|
| |
| Others Important Tips |
Always flood screen when completed every printing stroke, this is to prevent ink from drying on screen. **Avoid
printing detail immediately after flash curing Flash curing temperature required is 220 degree Celsius for not more
than 10 second at 2500 cfm flash curing heat air flow.
|
|
|
 |